| Item | Liquid forging(squeeze casting) | Forging | Counter-pressure casting | Low pressure casting | Gravity casting | High pressure casting |
| Surface quality | good | good | medium | medium | bad | good |
| Internal quality | formed under the pressure of about 100MPa, with fine grain and fine structure | Fine grain and fine structure under forging | formed under the pressure of about 0.6 MPa, with coarse grain and loose structure | formed under the pressure of about 0.01-0.05 MPa, with coarse grains and loose structure | filled and formed by its own weight, with very coarse grains and loose organization | High speed water spraying, no feeding, many internal pores and loose structure |
| Surface roughness | Ra3.2-1.6 | Ra3.2-1.6 | Ra6.3-3.2 | Ra6.3-3.2 | Ra6.3-3.2 | Ra3.2-1.6 |
| Heat treatment | Solid solution(T6) | Solid solution(T6) | Solid solution(T6) | Solid solution(T6) | Solid solution(T6) | no |
| Production efficiency | High | Low | Medium | Medium | Low | High |
| Forming accuracy | High lever of one-time forming and less machining allowance | Low lever of one-time forming , the process is complex, and a lot of subsequent processing is required | A lot of subsequent processing is required | A lot of subsequent processing is required | A lot of subsequent processing is required | High lever of one-time forming and less machining allowance |
| Mechanical properties | Close to forging level without forging streamline | Highest (but there is forging streamline, which makes the metal properties anisotropic) | Medium | Medium | Medium | Low |